The Steel Weights & pH 2/22/11:
A: 23.7g pH 8
B: 25.7g pH 11
C: 25.2g pH 12
D: 25.6g pH 6
E: 25.9g pH 6
F: 25.5g pH 4
The steel has corroded greatly, and it has shown most in the Clorox/chlorine. Though it is not the greatest weight change, it has the most apparent rust. The ammonia is still a dark blue, and the drano is clear. The least change came from the drano and ammonia. Even water had change. When dried, the metal each left a white residue that covered it totally. Sulfuric acid corroded the metal definitely, but it did it in a way that the metal did not have seen rust, but corroded the metal weight, and left the metal looking slightly shriveled.